Bar rownd dur 20NiCrMoS6-4 DIN 1.6571
Cyfansoddiad cemegol % y dadansoddiad ladle o radd dur:20NiCrMoS6-4
| 0.16-0.23 | Uchafswm 0.40 | 0.50-0.90 | Uchafswm 0.035 | 0.020-0.040 | 0.60-0.90 |
| 1.40-1.70 | 0.25-0.35 | ||||
Proses: EAF+LF+VD+Forged Treatment(optional)
YSTOD MAINT:
Crwn:
Hot Forged: 50mm-2000mm
Fflat:
Hot Forged: Trwch: Lled 50-600mm: hyd at 1600mm
GORFFENIADAU ARWYNEB:
Du, Wedi'i Droi a'i Grilio
Prawf: Prawf ultrasonic yn ôl SEP 1921-84 C / c, D / d, E/e
Triniaeth Gwres
Annealing, Normaleiddio, Quenching, Tymer
Priodweddau Mecanyddol
| Priodweddau | Amodau | ||
|---|---|---|---|
| T (°C) | Triniaeth | ||
| Dwysedd (×1000 kg/m3) | 7.7-8.03 | 25 | |
| Cymhareb Poisson | 0.27-0.30 | 25 | |
| Modulus Elastig (GPa) | 190-210 | 25 | |
| Cryfder Tynnol (Mpa) | 1158 | 25 | olew wedi'i quenched, grawn mân, wedi'i dymheru ar 425°C |
| Cryfder Cynnyrch (MPA) | 1034 | ||
| Huawdl (%) | 15 | ||
| Gostyngiad yn yr Ardal (%) | 53 | ||
| Caledwch (HB) | 335 | 25 | olew wedi'i quenched, grawn mân, wedi'i dymheru ar 425°C |
PRIODWEDDAU THERMOL
| Priodweddau | Amodau | ||
|---|---|---|---|
| T (°C) | Triniaeth | ||
| Dargludedd Thermal (W/m-K) | 42.7 | 100 | |
| Gwres Penodol (J/kg-K) | 477 | 50-100 | |
PRIODWEDDAU HYSICAL
| Maint | Gwerth | Uned |
|---|---|---|
| Ehangu thermol | 16 - 17 | e-6/K |
| Dargludedd thermol | 16 - 16 | W/m.K |
| Gwres penodol | 500 - 500 | J/kg. K |
| Tymheredd toddi | 1370 - 1400 | °C |
| Tymheredd y gwasanaeth | 0 - 500 | °C |
| Dwysedd | 8000 - 8000 | kg/m3 |
| Gwrthsefyll | 0.7 - 0.7 | Ohm.mm2/m |